| According with GB EZNiFe-1 Corresponding with AWS ENiFe-C1 | |||||||||||||||||
| Introduction: ENiFe-C1 is a kind of cast iron electrode with Ni-Fe alloy core wire and strong reducibility graphite type coating. It has some characteristics like high strength, good plasticity, low coefficient of linear expansion, etc. The crack-resistance for gray cast iron is similar with that of EZNi-1, but the crack-resistance for spheroidal graphite cast iron is higher than that of EZNi-1. It is also effective for cast iron with high phosphorus content (0.2%P). The machinability is a little worse than that of EZNi-1 and ENiCu-B. Used for welding gray cast iron and spheroidal graphite cast iron under normal temperature or preheated a little (to about 200℃). AC/DC. | |||||||||||||||||
| Uses: Suitable for repair welding on key high strength gray cast iron and spheroidal graphite cast iron, such as cylinders, engine bearers, gears, rollers, etc. | |||||||||||||||||
| Chemical Composition of Deposited Metal (%)
| |||||||||||||||||
| Reference Current(AC, DC+)
| |||||||||||||||||
| Instructions: The electrodes must be baked under about 150℃ for an hour before welding. | |||||||||||||||||
| According with GB EZNiFe-1 Corresponding with AWS ENiFe-C1 | |||||||||||||||||
| Introduction: ENiFe-C1 is a kind of cast iron electrode with Ni-Fe alloy core wire and strong reducibility graphite type coating. It has some characteristics like high strength, good plasticity, low coefficient of linear expansion, etc. The crack-resistance for gray cast iron is similar with that of EZNi-1, but the crack-resistance for spheroidal graphite cast iron is higher than that of EZNi-1. It is also effective for cast iron with high phosphorus content (0.2%P). The machinability is a little worse than that of EZNi-1 and ENiCu-B. Used for welding gray cast iron and spheroidal graphite cast iron under normal temperature or preheated a little (to about 200℃). AC/DC. | |||||||||||||||||
| Uses: Suitable for repair welding on key high strength gray cast iron and spheroidal graphite cast iron, such as cylinders, engine bearers, gears, rollers, etc. | |||||||||||||||||
| Chemical Composition of Deposited Metal (%)
| |||||||||||||||||
| Reference Current(AC, DC+)
| |||||||||||||||||
| Instructions: The electrodes must be baked under about 150℃ for an hour before welding. | |||||||||||||||||