| J707RH | According with GB E7015-G Corresponding with AWS E10015-G | |||||||||||||||||||||||||||
| Introduction: J707RH is a kind of super low hydrogen high toughness electrode with low-hydrogen natrium type coating. DCRP (Direct Current Reversed Polarity). All-position welding. It has excellent welding performance. The deposited metal has excellent plasticity and toughness. | ||||||||||||||||||||||||||||
| Uses: Used for welding hull structures, and also used for welding key high strength steel structures with σ0.2≥590MPa. | ||||||||||||||||||||||||||||
Chemical Composition of Deposited Metal (%)
| ||||||||||||||||||||||||||||
Mechanical Properties of Deposited Metal
| ||||||||||||||||||||||||||||
| Diffusible Hydrogen Content in Deposited Metal:≤4.1ml/100g(Chromatography or Mercury Method) | ||||||||||||||||||||||||||||
| X-ray Radiographic Inspection:ⅠDegree | ||||||||||||||||||||||||||||
Reference Current(DC+)
| ||||||||||||||||||||||||||||
| Instructions: 1.The electrodes must be baked under about 400℃ for 2 hours before welding, and used as soon as baking is completed. 2.The stains on the weldments, such as rust, oil stains, moisture, etc., must be cleared away before welding. 3.When welding, short arc must be used and stringer bead is suitable. | ||||||||||||||||||||||||||||
| J707RH | According with GB E7015-G Corresponding with AWS E10015-G | |||||||||||||||||||||||||||
| Introduction: J707RH is a kind of super low hydrogen high toughness electrode with low-hydrogen natrium type coating. DCRP (Direct Current Reversed Polarity). All-position welding. It has excellent welding performance. The deposited metal has excellent plasticity and toughness. | ||||||||||||||||||||||||||||
| Uses: Used for welding hull structures, and also used for welding key high strength steel structures with σ0.2≥590MPa. | ||||||||||||||||||||||||||||
Chemical Composition of Deposited Metal (%)
| ||||||||||||||||||||||||||||
Mechanical Properties of Deposited Metal
| ||||||||||||||||||||||||||||
| Diffusible Hydrogen Content in Deposited Metal:≤4.1ml/100g(Chromatography or Mercury Method) | ||||||||||||||||||||||||||||
| X-ray Radiographic Inspection:ⅠDegree | ||||||||||||||||||||||||||||
Reference Current(DC+)
| ||||||||||||||||||||||||||||
| Instructions: 1.The electrodes must be baked under about 400℃ for 2 hours before welding, and used as soon as baking is completed. 2.The stains on the weldments, such as rust, oil stains, moisture, etc., must be cleared away before welding. 3.When welding, short arc must be used and stringer bead is suitable. | ||||||||||||||||||||||||||||