ER70S-6
Mighty
72292000
| Quantity: | |
|---|---|
| Chemical Composition of Deposited Metal(%) | ||||||||
| | C | Mn | Si | S | P | Ni | Cr | Cu |
| Guaranteed Value | 0.06-0.15 | 1.4-1.85 | 0.8-1.15 | ≤0.030 | ≤0.030 | ≤0.15 | ≤0.15 | ≤0.5 |
| Typical Value | 0.08 | 1.52 | 0.89 | 0.019 | 0.018 | 0.013 | 0.016 | 0.15 |
| | Tensile Strength Rm(MPa) | Yield Strength ReL(MPa) | Elongation (%) | Test Temp (ºC) | Shielding gas | Absored Energy (J) |
| Sample Values | ≥500 | ≥420 | ≥22 | -30 | CO2 | ≥27 |
| Dia(mm) | φ 0.8 | φ 0.9 | φ 1.0 | φ 1.2 | φ 1.6 |
| Welding Current(A) | 50-100 | 50-110 | 50-220 | 80-350 | 170-550 |
| CO2 Flow Rate(L/MIN) | 15 | 15 | 15-20 | 15-25 | 20-25 |
| Chemical Composition of Deposited Metal(%) | ||||||||
| | C | Mn | Si | S | P | Ni | Cr | Cu |
| Guaranteed Value | 0.06-0.15 | 1.4-1.85 | 0.8-1.15 | ≤0.030 | ≤0.030 | ≤0.15 | ≤0.15 | ≤0.5 |
| Typical Value | 0.08 | 1.52 | 0.89 | 0.019 | 0.018 | 0.013 | 0.016 | 0.15 |
| | Tensile Strength Rm(MPa) | Yield Strength ReL(MPa) | Elongation (%) | Test Temp (ºC) | Shielding gas | Absored Energy (J) |
| Sample Values | ≥500 | ≥420 | ≥22 | -30 | CO2 | ≥27 |
| Dia(mm) | φ 0.8 | φ 0.9 | φ 1.0 | φ 1.2 | φ 1.6 |
| Welding Current(A) | 50-100 | 50-110 | 50-220 | 80-350 | 170-550 |
| CO2 Flow Rate(L/MIN) | 15 | 15 | 15-20 | 15-25 | 20-25 |