| A107 | According with GB E308-15 Corresponding with AWS E308-15 | ||||||||||||||||||||
| Introduction: A107 is a kind of Cr19Ni10 stainless steel electrode with basic coating. The weld metal has excellent mechanical properties and intercrystalline corrosion-resistance. DCRP (Direct Current Reversed Polarity). All-position welding. | |||||||||||||||||||||
| Uses: Used for welding corrosion-resistant 0Cr19Ni9 stainless steel structures below 300℃, and also used for weld some steel with worse weldability ( such as high-chrome steel, etc.) and surfacing welding on the surface layers of stainless steel. | |||||||||||||||||||||
| Chemical Composition of Deposited Metal (%)
| |||||||||||||||||||||
| Mechanical Properties of Deposited Metal
| |||||||||||||||||||||
| Reference Current(DC+)
| |||||||||||||||||||||
| Instructions: 1.The electrodes should be baked under about 250℃ for an hour before welding. 2.The stains on the weldments, such as oil stains, rust, moisture, etc., must be cleared away before welding. | |||||||||||||||||||||
| A107 | According with GB E308-15 Corresponding with AWS E308-15 | ||||||||||||||||||||
| Introduction: A107 is a kind of Cr19Ni10 stainless steel electrode with basic coating. The weld metal has excellent mechanical properties and intercrystalline corrosion-resistance. DCRP (Direct Current Reversed Polarity). All-position welding. | |||||||||||||||||||||
| Uses: Used for welding corrosion-resistant 0Cr19Ni9 stainless steel structures below 300℃, and also used for weld some steel with worse weldability ( such as high-chrome steel, etc.) and surfacing welding on the surface layers of stainless steel. | |||||||||||||||||||||
| Chemical Composition of Deposited Metal (%)
| |||||||||||||||||||||
| Mechanical Properties of Deposited Metal
| |||||||||||||||||||||
| Reference Current(DC+)
| |||||||||||||||||||||
| Instructions: 1.The electrodes should be baked under about 250℃ for an hour before welding. 2.The stains on the weldments, such as oil stains, rust, moisture, etc., must be cleared away before welding. | |||||||||||||||||||||