| A412 | According with GB E310Mo-16 Corresponding with AWS E310Mo-16 | ||||||||||||||||||||
| Introduction: A412 is a kind of Cr26Ni21Mo2 pure austenitic stainless steel electrode with lime-titania type coating. Due to Mo added to the weld metal, the corrosion-resistance, heat-resistance and crack-resistance are all better than those of A402 and A407. AC/DC. The welding performance is excellent. | |||||||||||||||||||||
| Uses: Used for welding heat-resistant stainless steel working under high temperatures, and also used for welding stainless steel lining, dissimilar steel, etc. When welding carbon steel and low-alloy steel with high hardenability, the toughness is extremely excellent. | |||||||||||||||||||||
| Chemical Composition of Deposited Metal (%)
| |||||||||||||||||||||
| Mechanical Properties of Deposited Metal
| |||||||||||||||||||||
| Reference Current(AC, DC+)
| |||||||||||||||||||||
| Instructions: 1.The electrodes should be baked under 200-250℃ for an hour before welding. 2.When welding, the current should not be too strong. | |||||||||||||||||||||
| A412 | According with GB E310Mo-16 Corresponding with AWS E310Mo-16 | ||||||||||||||||||||
| Introduction: A412 is a kind of Cr26Ni21Mo2 pure austenitic stainless steel electrode with lime-titania type coating. Due to Mo added to the weld metal, the corrosion-resistance, heat-resistance and crack-resistance are all better than those of A402 and A407. AC/DC. The welding performance is excellent. | |||||||||||||||||||||
| Uses: Used for welding heat-resistant stainless steel working under high temperatures, and also used for welding stainless steel lining, dissimilar steel, etc. When welding carbon steel and low-alloy steel with high hardenability, the toughness is extremely excellent. | |||||||||||||||||||||
| Chemical Composition of Deposited Metal (%)
| |||||||||||||||||||||
| Mechanical Properties of Deposited Metal
| |||||||||||||||||||||
| Reference Current(AC, DC+)
| |||||||||||||||||||||
| Instructions: 1.The electrodes should be baked under 200-250℃ for an hour before welding. 2.When welding, the current should not be too strong. | |||||||||||||||||||||