Standard conforming: GB/T5293-1999 F4A2-H08A Equivalent to : AWS A5.17 F6A0-EL12 Description and Applications SJ401 is a type of silicon and calcium based agglomerated flux, the chemical property of which is acidic, taupe to black spherical grains in appearance. Its grain size is 2.0-0.28mm(10-60meshes). Flux SJ401 is suitable for use with AC or DC power, filler wires connect with Positive Electrode while in DC. With excellent technical properties, the flux provides high resistant to stomata. Flux for welding of low carbon steels and some low alloy steels in combination with H08A, being used in locomotive vehicles, mining machinery and other structural applications. Machanical properties of Deposited Metal
Wire
Tensile Strength Rm(MPa)
Yield Strength Reh(MPa)
Elongation (A%)
AKV(J)
-20℃
H08A
415-550
≥330
≥22
≥27
Packing: 25kg per kraft paper bag or 1000kg per jumbo bag.
Remarks: 1. Redry the flux at 300-350℃ for 2hours before welding. 2. Impurities such as rust, greasy dirt, moisture, ect.should be cleared from the welding area.
SJ401 Agglomerated Flux for S.A. Welding
Standard conforming: GB/T5293-1999 F4A2-H08A Equivalent to : AWS A5.17 F6A0-EL12 Description and Applications SJ401 is a type of silicon and calcium based agglomerated flux, the chemical property of which is acidic, taupe to black spherical grains in appearance. Its grain size is 2.0-0.28mm(10-60meshes). Flux SJ401 is suitable for use with AC or DC power, filler wires connect with Positive Electrode while in DC. With excellent technical properties, the flux provides high resistant to stomata. Flux for welding of low carbon steels and some low alloy steels in combination with H08A, being used in locomotive vehicles, mining machinery and other structural applications. Machanical properties of Deposited Metal
Wire
Tensile Strength Rm(MPa)
Yield Strength Reh(MPa)
Elongation (A%)
AKV(J)
-20℃
H08A
415-550
≥330
≥22
≥27
Packing: 25kg per kraft paper bag or 1000kg per jumbo bag.
Remarks: 1. Redry the flux at 300-350℃ for 2hours before welding. 2. Impurities such as rust, greasy dirt, moisture, ect.should be cleared from the welding area.