Mighty(Qingdao) Metal Materials CO.,LTD
Tel:  +0086-532-66010296
Hot Search:  Welding electrodes for carbon steel      Welding electrodes for stainless steel 

Products Category

Contacts Us

c
Mighty(Qingdao) Metal Materials CO.,LTD
 Email: info@mightymetal.net
 Phone: +0086-53266010291/
66010292/66010293/66010296
 Fax: +0086-532-66010292
 Mobile Phone: 15066257152
 QQ: 718282180
 Address: Room No.705,Block A,Heda Central Plaza,No.175,Tailiu Road,Shibei District, Qingdao City,China
 

loading

Share to:
sharethis sharing button

SJ501

  • SJ501

  • Mighty

Quantity:
Specification: EN760 SA AR 1 88 AC H5
             AWS A5.17 F7A0-EL12 F7A2-EM12K

Application:
With suitable welding wires(H08MnA. H08MnMoA. H10Mn2), it can welding common structural steel, boiler steel, pipeline steel, etc.
The flux can be used for multiple fast welding, and can be suitable for single-sided welding, especially suitable for pressure vessel, such as oil and gas pipes, tanks and cylinders of
 automatic submerged arc welding.

Description:
     Agglomerated flux SJ501 is a kind of acid aluminum-titanium type sintered flux, the basicity index is
about 0.8. It is shaped as black, round grains and its grain size is 2.0-0.28mm (10-60Mesh). It can be
used with either AC or DC. The welding wire is connected to the positive electrode when used with DC.
It has stable combustion, good slag detachability and good appearance of weld. It has a thick skin to
a small quality of rust and high temperature oxidation film on account of strong the capability of resist
pore.
      As a peculiar production technique is adopted, the flux possesses better moisture resistance and good strength of grains,
which may satisfy the requirements for regular transportation, storage and recycling
 use in welding.
The flux has less specific gravity when it is bulk packed. And it is consumed less during
 the welding.
 
Cautions:
1.The oil contamination, moisture, iron rust and other foreign substances must be removed from the
welding joint.
2. It is better to weld under direct current.
3. Welding flux must be baked under 300-350°C for more than 2hours before usage.
 
Chemical Compositions:
Al2O3+MnO CaO+MgO SiO2+TiO2 CaF2 S P
25~30 25~30 15~20 15~20 ≤0.03 ≤0.03
(Mechanical Performance of the Deposited Metal):
Wires Standard Models бs(Mpa) бb(Mpa) δ5 Akv(J)
HO8A F4A2-HO8A ≥330 ≥420 ≥22% ≥27
HO8MnA F5A2-HO8MnA ≥400 ≥500 ≥22% ≥27
 
Mechanical Property:(according to GB5293-1999 F4A1-H08A)
Test Item Tensile Strength
(MPa)
Yield Strength 
(MPa)
Elongation 
(%)
Impact Value(J)
-40°C
Guaranteed Value 410~550 ≥330 ≥22 ≥27

Previous: 
Next: 

Mighty(Qingdao) Metal Materials CO.,LTD

Address: Room No.705,Block A,Heda Central Plaza,No.175,Tailiu Road,Shibei District, Qingdao City,China
Phone: +0086-532-66010291/66010292/66010293/66010296
Email: info@mightymetal.net
Home
Copyright  2016 Mighty(Qingdao) Metal Materials CO.,LTD.All rights reserved, Supportded by Leadong